Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Ultramid T - PA-Cop - BASF

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Ultramid T" in Material Data Center leads to the following information:

Tradename: Ultramid T
Family: PA-Cop
Producer: BASF
13 hits in the material database
7 hits in the literature database
5 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Application
Ultramid® T KR 4355 G7 Fuel tank sensor
Ultramid® T 4381 LDS 3D moulded interconnected device
Ultramid® T KR 4357 G6 Quick connectors, fuel pipes
Ultramid® T 4381 LDS Interconnect devices, MID
Ultramid® T KR 4355 G10 Valve body, fire extinguisher

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.